top of page

Optimizing Charge/Discharge Protocol for Early-Cycle Degradation in Lithium Metal Batteries

Allen Liu
26/10/2026

Lithium metal anodes are often considered the "holy grail" of rechargeable, sustainable battery technology. With the highest theoretical specific capacity (3,860 mAh g⁻¹) and lowest electrochemical potential (−3.04 V vs. standard hydrogen electrode) of any metallic element, they represent the clearest path toward the next generation of higher-energy-density batteries in electric vehicles, consumer electronics, and medical devices. Their commercial adoption, however, is limited by uncontrolled lithium dendritic growth during electrochemical cycling.

This study investigates how operating temperature (room temperature vs. 35°C) and depth of discharge (DoD; Low vs. Full) influence dendrite-related degradation in Li-NMC811 CR2032 coin cells. Electrochemical impedance spectroscopy (EIS) was used to track changes in Ohmic, SEI, and charge-transfer resistance. Voltage-profile analysis and Coulombic efficiency measurements across cycling further capture how these conditions affect rate capability and the reversibility of capacity loss over time. This study seeks to move dendrite mitigation beyond the materials-level fixes that have dominated the field, toward practical, low-cost charging protocols that could be the deciding factor in whether lithium metal batteries become safe and reliable enough for widespread, real-world use.

bottom of page